PDF p. 1713 · 9-19
| All Paint | Painting of complete surface. |
| Air blow | Using compressed air to blow away dust and debris. |
| Block paint | Painting a section only, such as a door. |
| Clear paint (clear coat) | Clear paint without dye (pigment). |
| Double coat | Application of two paint coats. |
| Dry coat | Paint which left the spray gun and dried partially before it reached the surface, thereby making the painted surface rough. Dry coating is |
| caused by too little paint being fed, too high an air pressure, too much distance between the painted surface and the gun, or moving the gun | |
| too fast. | |
| Dry film | Paint which has dried completely. |
| Dust coat | Paint is applied thinner than a dry coat. Painted surface becomes rough. |
| ED painting | Electrostatic discharge painting. |
| Enamel | Finishing paint pigmented with dye. |
| Featheredging | Smoothing off the edges of painted surfaces. |
| Flash off | Evaporation of the paint solvent. (Flash off time is the period between paint coat applications). |
| Ford cup | A type of viscosity meter. |
| Gun stroke | Movement of the paint gun. |
| Hardener | Hardening agent of two-liquid type paint or fillers. |
| Polycyanates and oxides are used for hardeners. | |
| Heat-hardening acrylic resin paint | Composed of acrylic resin and meramine resin, and hardened (forms a paint film) by baking. |
PDF p. 1714 · 9-20
| Lacquer | A type of paint that uses cellulose nitrate or other chemicals, and which dries by evaporation of its solvent agent. |
| Meramine resin | Used as component for aminoalkyd resin paint and heat-hardening acrylic resin paint. |
| Metallic-base paint | Paint with aluminium powder for metallic tone. |
| Mist coat | Painting for fade-in sections. A small amount of paint may be dissolved with slow-evaporating thinner, or thinner alone may be applied with |
| low pressure 150 - 200 kPa (1.5 - 2.0 kgf/cm2, 21.3 - 28.4 psi). | |
| Mixing scale | Colour mixing device. |
| Overlap | Blending of spray patterns. |
| Overspray | Spraying other than the area that needs painting. |
| Paddle | A tool to mix paint |
| Paint dust | Dust of paint formed by spraying |
| Paper dispenser | A paper posting device (masker) that combines tape and paper. |
| Scrapes | Traces of scratches. |
| Scuffing | Particles on the painted surface are lightly polished with fine emery paper (#600 or over). |
| Set (setting) | Evaporation time of solvent in the paint, before drying the layer forcefully or by baking (May be considered the same as flash-off time). |
| Single coat | Application of paint in single layer. |
| Spot paint | Painting of small section, such as for touch-up. |
| Undercoat | Undercoat paint (such as primer and surfacer). |
May be applied to lower section of car for noise prevention and rustproofing.
PDF p. 1715 · 9-21
| Wet coat | Paint is applied with an excess of solvent, thereby producing a painted surface that is smooth, glossy and has a wet look. |
| Wet film | Paint which has not dried completely. |
| Wet on wet | Application of the next coat of paint before the preceding layer has dried completely. |
| Wool bonnet | Wool grinder for compound polishing. |